Posted by colinhester [ 65.27.134.38 ] on August 18, 2006 at 20:38:00:

In Reply to: Re: Yeap posted by 2wo on August 18, 2006 at 17:53:23:

Making an electrical connection to each pin would not be trivial. This connection would oxidize (disolve) before the gold plating.

Using cyanide in a lab setting is actually pretty safe. If that scares you, look at "Aqua Regia." This scares the crap out of me....